[an error occurred while processing this directive]
SiCf/Ti65复合材料界面反应与基体相变机理
王超1,2, 张旭1(), 王玉敏1(), 杨青1, 杨丽娜1, 张国兴1, 吴颖1, 孔旭1, 杨锐1
Mechanisms of Interfacial Reaction and Matrix Phase Transition in SiCf /Ti65 Composites
WANG Chao1,2, ZHANG Xu1(), WANG Yumin1(), YANG Qing1, YANG Lina1, ZHANG Guoxing1, WU Ying1, KONG Xu1, YANG Rui1

图3. SiCf /Ti65复合材料成型态界面区域的SEM像和EDS元素面分布图
Color online

Fig.3. SEM image and EDS elemental mapping in the fiber/matrix interfacial reaction zone for the as-processed SiCf /Ti65 composites