[an error occurred while processing this directive]
非等温时效对7B50铝合金组织及性能的影响
李吉臣1, 冯迪1,2(), 夏卫生2, 林高用3, 张新明3, 任敏文1
Effect of Non-Isothermal Ageing on Microstructure and Properties of 7B50 Aluminum Alloy
LI Jichen1, FENG Di1,2(), XIA Weisheng2, LIN Gaoyong3, ZHANG Xinming3, REN Minwen1

图7. 7B50铝合金非等温时效过程中的Scheil积分-升温时间关系曲线

Fig.7. Scheil integral-heating time curve of 7B50 aluminum alloy during non-isothermal heating ageing (S—Scheil integral value of different ageing schedules, Sc—Scheil integral value of a reference ageing schedule)