电磁搅拌对TiB2颗粒增强钢组织和力学性能的影响
张林1, 郭晓1,2, 高建文1, 邓安元1, 王恩刚1()
Effect of Electromagnetic Stirring on Microstructure and Mechanical Properties of TiB2 Particle-Reinforced Steel
ZHANG Lin1, GUO Xiao1,2, GAO Jianwen1, DENG Anyuan1, WANG Engang1()

图8. 磁场对Fe-TiB2颗粒增强钢熔体及颗粒的驱动作用示意图及α值变化趋势

Fig.8. Schematic of driving effect of magnetic field (B) on the melt of Fe-TiB2 particle-reinforced steel (a), and α value change with melt temperature and particle size (b)