电磁搅拌对TiB2颗粒增强钢组织和力学性能的影响
张林1, 郭晓1,2, 高建文1, 邓安元1, 王恩刚1()
Effect of Electromagnetic Stirring on Microstructure and Mechanical Properties of TiB2 Particle-Reinforced Steel
ZHANG Lin1, GUO Xiao1,2, GAO Jianwen1, DENG Anyuan1, WANG Engang1()

图2. 有无电磁搅拌作用下TiB2颗粒增强钢的XRD谱

Fig.2. XRD spectra of TiB2 particle-reinforced steel with and without electromagnetic stirring (EMS)