固溶温度对Fe-19Mn合金的γ→ε相变和阻尼性能的影响
王世宏, 李健(), 柴锋, 罗小兵, 杨才福, 苏航
Influence of Solution Temperature on γ→ε Transformation and Damping Capacity of Fe-19Mn Alloy
WANG Shihong, LI Jian(), CHAI Feng, LUO Xiaobing, YANG Caifu, SU Hang

图5. 奥氏体晶粒尺寸和γ→ε相变开始温度(Msγ→ε)随固溶温度的变化

Fig.5. Variations of austenite grain size and Msγ→ε with solution temperature (Msγ→ε—starting temperature of γ→ε transformation)