固溶温度对Fe-19Mn合金的γ→ε相变和阻尼性能的影响
王世宏, 李健(), 柴锋, 罗小兵, 杨才福, 苏航
Influence of Solution Temperature on γ→ε Transformation and Damping Capacity of Fe-19Mn Alloy
WANG Shihong, LI Jian(), CHAI Feng, LUO Xiaobing, YANG Caifu, SU Hang

图4. 固溶温度对ε-马氏体板条尺寸和γ/ε相界面相对长度的影响

Fig.4. The influence of solution temperature on ε-mar-tensite plate size (a) and relative length of γ/ε interface (b)