航空发动机整体叶环中纤维断丝超声检测方法
武玉鹏1,2, 张博1(), 李经明1, 张双楠1, 吴颖1, 王玉敏1, 蔡桂喜1
Ultrasonic Detection for Fiber Broken in Aero-Engine Integral Bladed Ring
WU Yupeng1,2, ZHANG Bo1(), LI Jingming1, ZHANG Shuangnan1, WU Ying1, WANG Yumin1, CAI Guixi1

图3. 一种特殊纵波P1入射形成的头波系统[23]

Fig.3. A head wave system formed by the incidence of a special longitudinal wave P1 (λ, μ—elastic constants; ρ—density; S—shear wave, P—longitudinal wave; CL—P-wave velocity, CS—shear wave velocity; 1—mediume Ⅰ, 2—mediume Ⅱ; point S—hypocenter; i1—first critical angle; point C(r, z)—arbitrary position on the wavefront in the first medium, r—the horizontal distance from point C to the source; z—vertical distance from point C to the interface)[23]