航空发动机整体叶环中纤维断丝超声检测方法
武玉鹏1,2, 张博1(), 李经明1, 张双楠1, 吴颖1, 王玉敏1, 蔡桂喜1
Ultrasonic Detection for Fiber Broken in Aero-Engine Integral Bladed Ring
WU Yupeng1,2, ZHANG Bo1(), LI Jingming1, ZHANG Shuangnan1, WU Ying1, WANG Yumin1, CAI Guixi1

图15. 带预制纤维断丝缺陷的Ti-MMC试样

Fig.15. Ti-MMC specimen with the defect of fiber fracture (unit: mm) (a) front view (b) left view
Color online