连铸圆坯非均匀传热/凝固行为的无网格计算方法
|
|
Meshless Method for Non-Uniform Heat Transfer/Solidification Behavior of Continuous Casting Round Billet
|
|
图11. 弯月面下75 mm、285 mm和结晶器出口的周向热流和坯壳厚度以及平均热流与出口处坯壳厚度的对比 |
Fig.11. Comparisons of the circumferential heat flux with the shell thickness at mold height of 75 mm (a) and 285 mm (b), and mold outlet (c), and the comparison of averaged heat flux along the casting direction with the shell thickness (d) |
![]() |