[an error occurred while processing this directive]
连铸圆坯非均匀传热/凝固行为的无网格计算方法
蔡来强1,2, 王旭东1,2(), 姚曼1,2, 刘宇3
Meshless Method for Non-Uniform Heat Transfer/Solidification Behavior of Continuous Casting Round Billet
CAI Laiqiang1,2, WANG Xudong1,2(), YAO Man1,2, LIU Yu3

图10. 热流、坯壳表面温度和坯壳厚度沿浇铸方向的对比

Fig.10. Heat flux (a), predicted shell surface temperature (b) and shell thickness (c) along the casting direction at different angles