连铸圆坯非均匀传热/凝固行为的无网格计算方法
蔡来强1,2, 王旭东1,2(), 姚曼1,2, 刘宇3
Meshless Method for Non-Uniform Heat Transfer/Solidification Behavior of Continuous Casting Round Billet
CAI Laiqiang1,2, WANG Xudong1,2(), YAO Man1,2, LIU Yu3

图2. 热电偶安装示意图和热流传感器结构示意图

Fig.2. Schematics of the mold assembly (a) and structure of heat flux sensor (b) (T1 and T2 are the temperatures measured by two thermocouples; R1 and R2 are the distances from the two thermocouples to the hot surface of the mold)