[an error occurred while processing this directive]
31%B4Cp/6061Al复合材料的热变形及加工图的研究
周丽1, 李明1, 王全兆2(), 崔超3, 肖伯律2, 马宗义2
Study of the Hot Deformation and Processing Map of 31%B4Cp/6061Al Composites
ZHOU Li1, LI Ming1, WANG Quanzhao2(), CUI Chao3, XIAO Bolv2, MA Zongyi2

图10. 31%B4Cp/6061Al复合材料在475 ℃、10 s-1热压缩条件下不同区域显微组织的OM像

Fig.10. OM images of 31%B4Cp/6061Al composites at temperature of 475 ℃ and strain rate of 10 s-1 at areas A (a), B (b) and C (c) in Fig.9