31%B4Cp/6061Al复合材料的热变形及加工图的研究
周丽1, 李明1, 王全兆2(), 崔超3, 肖伯律2, 马宗义2
Study of the Hot Deformation and Processing Map of 31%B4Cp/6061Al Composites
ZHOU Li1, LI Ming1, WANG Quanzhao2(), CUI Chao3, XIAO Bolv2, MA Zongyi2

图6. 31%B4Cp/6061Al复合材料在不同应变下的失稳图

Fig.6. Instability zones of 31%B4Cp/6061Al composites at strains of 0.1 (a), 0.3 (b), 0.5 (c) and 0.7 (d) (The contours represent instability factors (ξ), and the blue regions less than zero are the unstable regions, while the yellow regions greater than or equal to zero are the stable regions)