一种原子尺度应变定义方法及其在识别微观缺陷演化中的应用
盛鹰1,2, 贾彬1,2(), 王汝恒1,2, 陈国平1,2
The Definition of Atomic Scale Strain and Its Application in Identifying the Evolution of Microdefects
SHENG Ying1,2, JIA Bin1,2(), WANG Ruheng1,2, CHEN Guoping1,2

图2. NiTi合金三点弯曲试样断口形貌的SEM像

Fig.2. Low (a) and high (b) magnified fracture surface SEM images of three point bending NiTi alloy specimens