Ti-6Al-4V合金β→α相变中晶界α相形成机制的相场模拟
孙佳1,2, 李学雄1, 张金虎1, 王刚3, 杨梅4, 王皞1,5, 徐东生1,5()
Phase Field Modeling of Formation Mechanism of Grain Boundary Allotriomorph in β→α Phase Transformation in Ti-6Al-4V Alloy
SUN Jia1,2, LI Xuexiong1, ZHANG Jinhu1, WANG Gang3, YANG Mei4, WANG Hao1,5, XU Dongsheng1,5()

图3. 模拟组织(图1d)局部放大图及沿AB线的Al和V的浓度分布

Fig.3. Local zoomed-in view of microstructure in Fig.1d (a) and the corresponding concentration profiles of Al and V along the line AB (b)