打印参数对电子束增材制造Ti-Ni合金性能的影响
任德春1,2, 张慧博1, 赵晓东3, 王福雨4, 侯文韬1, 王绍钢1, 李述军1, 金伟1(), 杨锐1
Influence of Manufacturing Parameters on the Properties of Electron Beam Melted Ti-Ni Alloy
REN Dechun1,2, ZHANG Huibo1, ZHAO Xiaodong3, WANG Fuyu4, HOU Wentao1, WANG Shaogang1, LI Shujun1, JIN Wei1(), YANG Rui1

图5. EBM制备Ti-Ni合金样品的室温压缩应力-应变曲线

Fig.5. Compression stress-strain curves for EBMed Ti-Ni alloy samples fabricated with different manufacturing parameters at room temperature