[an error occurred while processing this directive]
打印参数对电子束增材制造Ti-Ni合金性能的影响
任德春1,2, 张慧博1, 赵晓东3, 王福雨4, 侯文韬1, 王绍钢1, 李述军1, 金伟1(), 杨锐1
Influence of Manufacturing Parameters on the Properties of Electron Beam Melted Ti-Ni Alloy
REN Dechun1,2, ZHANG Huibo1, ZHAO Xiaodong3, WANG Fuyu4, HOU Wentao1, WANG Shaogang1, LI Shujun1, JIN Wei1(), YANG Rui1

图8. EBM制备Ti-Ni合金样品S5的表面形貌、显微组织和EDS分析

Fig.8. SEM images of top surface (a), low (b) and high (c) magnified microstructures of top surface for building plane, SEM images of side surface (d), low (e) and high (f) magnified microstructures of side surface for building direction plane and SEM image before corrosion for building direction plane (g) for EBMed Ti-Ni alloy sample S5, and EDS results for positions 1~4 in Fig.8g (h, i)