[an error occurred while processing this directive]
打印参数对电子束增材制造Ti-Ni合金性能的影响
任德春1,2, 张慧博1, 赵晓东3, 王福雨4, 侯文韬1, 王绍钢1, 李述军1, 金伟1(), 杨锐1
Influence of Manufacturing Parameters on the Properties of Electron Beam Melted Ti-Ni Alloy
REN Dechun1,2, ZHANG Huibo1, ZHAO Xiaodong3, WANG Fuyu4, HOU Wentao1, WANG Shaogang1, LI Shujun1, JIN Wei1(), YANG Rui1

图7. EBM制备不同Ti-Ni合金样品的显微组织

Fig.7. Morphologies after compression testing (a, d, g), SEM images for whole fracture surface (b, e, h) and locally magnified SEM images for fracture surface (c, f, i) for EBMed Ti-Ni alloy samples S1 (a~c), S5 (d~f) and S7 (g~i)