打印参数对电子束增材制造Ti-Ni合金性能的影响
任德春1,2, 张慧博1, 赵晓东3, 王福雨4, 侯文韬1, 王绍钢1, 李述军1, 金伟1(), 杨锐1
Influence of Manufacturing Parameters on the Properties of Electron Beam Melted Ti-Ni Alloy
REN Dechun1,2, ZHANG Huibo1, ZHAO Xiaodong3, WANG Fuyu4, HOU Wentao1, WANG Shaogang1, LI Shujun1, JIN Wei1(), YANG Rui1

图6. EBM制备不同Ti-Ni合金样品的显微硬度及样品S5沿打印方向平面和打印平面上表面的显微硬度

Fig.6. Vickers hardnesses of EBMed Ti-Ni alloy samples with different manufacturing parameters (a) and sample S5 along the building direction plane and building plane on a straight testing line that spans the entire for ten different positions (b)