表5 扩散偶参数计算结果
Table 5 The calculation results of various parameters for Cu/HEA/304SS

Temperature

℃

Diffusion couple

ΔHmix

(kJ·mol-1)

δ

%

VEC

ΔSmix

(J·K-1·mol-1)

Phase
800Cu/HEA side2.082.78.5712.26fcc
HEA/304SS side-3.442.98.0413.03fcc
850Cu/HEA side0.482.78.4912.54fcc
HEA/304SS side-3.602.88.0113.13fcc
900Cu/HEA side1.152.58.5212.40fcc
HEA/304SS side-3.452.98.0113.08fcc