CoCrFeMnNi高熵合金作为中间层的Cu/304不锈钢扩散连接研究
丁文, 王小京, 刘宁, 秦亮

Diffusion Bonding of Copper and 304 Stainless Steel with an Interlayer of CoCrFeMnNi High-Entropy Alloy
DING Wen, WANG Xiaojing, LIU Ning, QIN Liang
表4 扩散偶不同区域的元素含量
Table 4 Chemical compositions of different regions of diffusion couple

Temperature

℃

Diffusion coupleElement composition (atomic fraction / %)
CoCrFeMnNiCu
800Cu/HEA side16.016.716.115.716.519.0
HEA/304SS side17.216.032.316.717.8-
850Cu/HEA side17.517.915.814.720.114.0
HEA/304SS side16.318.230.216.418.9-
900Cu/HEA side19.019.017.611.018.415.0
HEA/304SS side17.716.631.317.417.0-