时效路径对Al-0.7Mg-0.5Si-0.2Cu-0.5Zn合金沉淀析出行为的影响 |
||||||||||||
| 朱亮, 郭明星, 袁波, 庄林忠, 张济山 | ||||||||||||
|
Effect of Ageing Routes on Precipitation Behaviors of Al-0.7Mg-0.5Si-0.2Cu-0.5Zn Alloy |
||||||||||||
| ZHU Liang, GUO Mingxing, YUAN Bo, ZHUANG Linzhong, ZHANG Jishan | ||||||||||||
| 表1 不同时效路径处理后Al-0.7Mg-0.5Si-0.2Cu-0.5Zn合金峰时效态拉伸力学性能 |
||||||||||||
| Table 1 Tensile mechanical properties of Al-0.7Mg-0.5Si-0.2Cu-0.5Zn alloys in peak ageing state under different ageing processes |
||||||||||||
|
||||||||||||