[an error occurred while processing this directive]
时效路径对Al-0.7Mg-0.5Si-0.2Cu-0.5Zn合金沉淀析出行为的影响
朱亮1, 郭明星1,2(), 袁波1, 庄林忠1,2, 张济山1,2
Effect of Ageing Routes on Precipitation Behaviors of Al-0.7Mg-0.5Si-0.2Cu-0.5Zn Alloy
ZHU Liang1, GUO Mingxing1,2(), YUAN Bo1, ZHUANG Linzhong1,2, ZHANG Jishan1,2

图7. 时效路径对Al-0.7Mg-0.5Si-0.2Cu-0.5Zn合金沉淀相析出的影响模型图

Fig.7. Schematics of precipitation in the Al-0.7Mg-0.5Si-0.2Cu-0.5Zn alloy treated by the ageing routes
(a) AQ (b) AQ+short time ageing (c) AQ+peak ageing (d) PA (e) PA+short time ageing (f) PA+peak ageing