时效路径对Al-0.7Mg-0.5Si-0.2Cu-0.5Zn合金沉淀析出行为的影响
朱亮1, 郭明星1,2(), 袁波1, 庄林忠1,2, 张济山1,2
Effect of Ageing Routes on Precipitation Behaviors of Al-0.7Mg-0.5Si-0.2Cu-0.5Zn Alloy
ZHU Liang1, GUO Mingxing1,2(), YUAN Bo1, ZHUANG Linzhong1,2, ZHANG Jishan1,2

图1. Al-0.7Mg-0.5Si-0.2Cu-0.5Zn合金固溶淬火态和预时效态的DSC曲线

Fig.1. DSC curves of Al-0.7Mg-0.5Si-0.2Cu-0.5Zn alloys in the as-quenched and pre-aged conditions