难变形高温合金GH4975的铸态组织及均匀化
|
|
As-Cast Microstructure Characteristic and Homogenization of a Newly Developed Hard-Deformed Ni-Based Superalloy GH4975
|
|
图 5. 铸态GH4975热压缩试样中的碳化物形貌 |
Fig.5. The morphologies of MC carbide in the as-cast GH4975 samples after hot deformation (1160 ℃, 30%, 0.1 s-1) |
![]() |