[an error occurred while processing this directive]
难变形高温合金GH4975的铸态组织及均匀化
向雪梅, 江河(), 董建新, 姚志浩
As-Cast Microstructure Characteristic and Homogenization of a Newly Developed Hard-Deformed Ni-Based Superalloy GH4975
XIANG Xuemei, JIANG He(), DONG Jianxin, YAO Zhihao

图3. 铸态GH4975合金DSC加热曲线

Fig.3. DSC heating curve of as-cast GH4975 alloy