Ti-43.5Al-4Nb-1Mo-0.1B合金的包套热挤压组织与拉伸性能
|
|
Microstructure and Tensile Properties of Ti-43.5Al-4Nb-1Mo-0.1B Alloy Processed by Hot Canned Extrusion
|
|
图2. 挤压态与时效态TNM合金不同位置的微观组织BSE-SEM像 |
Fig.2. BSE-SEM images of microstructure of edge (a, c) and center (b, d) partitions of extrusion (a, b) and ageing (c, d) TNM alloys |
![]() |