[an error occurred while processing this directive]
二次枝晶取向对镍基高温合金晶粒竞争生长行为的影响
张小丽1, 冯丽2, 杨彦红3, 周亦胄3, 刘贵群1()
Influence of Secondary Orientation on Competitive Grain Growth of Nickel-Based Superalloys
ZHANG Xiaoli1, FENG Li2, YANG Yanhong3, ZHOU Yizhou3, LIU Guiqun1()

图7. θGB随二次晶界角的变化规律

Fig.7. Dependence of θGB on secondary grain boundary angle in the cases of convergence and divergence