二次枝晶取向对镍基高温合金晶粒竞争生长行为的影响
张小丽1, 冯丽2, 杨彦红3, 周亦胄3, 刘贵群1()
Influence of Secondary Orientation on Competitive Grain Growth of Nickel-Based Superalloys
ZHANG Xiaoli1, FENG Li2, YANG Yanhong3, ZHOU Yizhou3, LIU Guiqun1()

图3. 一次枝晶取向相同时双晶的纵截面和横截面组织

Fig.3. Macrographs showing the macrostructures on the longitudinal section (a) and top cross section (b) and OM image showing the microstructure on cross section (c) in Exp.1-9 (a1, a2—dendrites)