Al、Ni对1Cr9Al(1~3)Ni(1~7)WVNbB钢热变形行为的影响
赵嫚嫚1, 秦森1, 冯捷1, 代永娟1, 国栋1,2()
Effect of Al and Ni on Hot Deformation Behavior of 1Cr9Al(1~3)Ni(1~7)WVNbB Steel
ZHAO Manman1, QIN Sen1, FENG Jie1, DAI Yongjuan1, GUO Dong1,2()

图6. No.4试样lnσp-lnε˙、σp-lnε˙、ln[sinh(ασp)]-lnε˙、ln[sinh(ασp)]-1000/T的关系曲线

Fig.6. Relationship curves of sample No.4 with respect to lnσp-lnε˙ (a), σp-lnε˙ (b), ln[sinh(ασp)]-lnε˙ (c) and ln[sinh(ασp)]-1000/T (d) (α—stress level parameter)