Al、Ni对1Cr9Al(1~3)Ni(1~7)WVNbB钢热变形行为的影响
赵嫚嫚1, 秦森1, 冯捷1, 代永娟1, 国栋1,2()
Effect of Al and Ni on Hot Deformation Behavior of 1Cr9Al(1~3)Ni(1~7)WVNbB Steel
ZHAO Manman1, QIN Sen1, FENG Jie1, DAI Yongjuan1, GUO Dong1,2()

图5. 1Cr9Al(1~3)Ni(1~7)WVNbB高铝钢和T92钢[9]在不同变形温度和应变速率下的三维峰值流变应力图

Fig.5. Three-dimensional peak flow stress diagrams at different deformation temperatures and strain rates of samples No.1 (a), No.2 (b), No.3 (c), No.4 (d) and T92 steel[9] (e)