Al、Ni对1Cr9Al(1~3)Ni(1~7)WVNbB钢热变形行为的影响
赵嫚嫚1, 秦森1, 冯捷1, 代永娟1, 国栋1,2()
Effect of Al and Ni on Hot Deformation Behavior of 1Cr9Al(1~3)Ni(1~7)WVNbB Steel
ZHAO Manman1, QIN Sen1, FENG Jie1, DAI Yongjuan1, GUO Dong1,2()

图2. 合金钢理想状态下的真应力-真应变曲线

Fig.2. True stress-ture strain curves of alloy steel under ideal conditions (σp—peak flow stress; εp—strain under peak stress; I—work hardening stage; Ⅱ—dynamic recovery stage; Ⅲ—the dynamic recrystallization stage; Ⅳ—stable stage)