Al、Ni对1Cr9Al(1~3)Ni(1~7)WVNbB钢热变形行为的影响
赵嫚嫚, 秦森, 冯捷, 代永娟, 国栋

Effect of Al and Ni on Hot Deformation Behavior of 1Cr9Al(1~3)Ni(1~7)WVNbB Steel
ZHAO Manman, QIN Sen, FENG Jie, DAI Yongjuan, GUO Dong
表2 峰值应力下1Cr9Al(1~3)Ni(1~7)WVNbB高铝钢本构方程参数
Table 2 Parameters of the constitutive equation of 1Cr9Al-(1~3)Ni(1~7)WVNbB high aluminum steel under peak stress

Steel

No.

n

α

MPa-1

A

s-1

Q

kJ·mol-1

16.695210.007596.38581×1020531.825
26.324100.007153.99328×1017458.873
35.758050.007241.51538×1019492.812
44.432330.010605.67709×1016430.874