Mn对23%Cr节Ni型双相不锈钢高温拉伸行为的影响
邓亚辉, 杨银辉(), 蒲超博, 倪珂, 潘晓宇
Effect of Mn Addition on High Temperature Tensile Behavior of 23%Cr Low Nickel Type Duplex Stainless Steel
DENG Yahui, YANG Yinhui(), PU Chaobo, NI Ke, PAN Xiaoyu

图5. 不同Mn含量双相不锈钢试样在不同温度下拉伸时的抗拉强度和断面收缩率

Fig.5. Tensile strength (a) and reduction of area (b) at different tensile temperatures for the duplex stainless steel samples with different Mn additions