Mn对23%Cr节Ni型双相不锈钢高温拉伸行为的影响
邓亚辉, 杨银辉(), 蒲超博, 倪珂, 潘晓宇
Effect of Mn Addition on High Temperature Tensile Behavior of 23%Cr Low Nickel Type Duplex Stainless Steel
DENG Yahui, YANG Yinhui(), PU Chaobo, NI Ke, PAN Xiaoyu

图1. 不同Mn含量双相不锈钢试样在应变速率0.01 s-1下不同温度高温拉伸时的真应力-真应变曲线

Fig.1. True stress-true strain curves of different Mn addition duplex stainless steel samples tensiled at strain rate 0.01 s-1 under di?erent temperatures(a) 6.26%Mn(b) 10.27%Mn(c) 14.13%Mn