1100 MPa级高强钢的低周疲劳行为
周红伟1,2, 白凤梅3,4(), 杨磊1,2, 陈艳1,2, 方俊飞1,2, 张立强3, 衣海龙4, 何宜柱1,2
Low-Cycle Fatigue Behavior of 1100 MPa Grade High-Strength Steel
ZHOU Hongwei1,2, BAI Fengmei3,4(), YANG Lei1,2, CHEN Yan1,2, FANG Junfei1,2, ZHANG Liqiang3, YI Hailong4, HE Yizhu1,2

图3. 1100 MPa级高强钢的低周疲劳寿命曲线及与其它级别钢的低周疲劳寿命比较

Fig.3. The low-cycle fatigue curves of high-strength steels
(a) Manson-Coffin equation fitting curve for 1100 MPa grade steel(b) comparison of the LCF curves of several high-strength steels