热镀锌工艺中锌液表面流速的在线电磁测量
郑锦灿, 刘润聪(), 王晓东()
Online Electromagnetic Measurement of Molten Zinc Surface Velocity in Hot Galvanized Process
ZHENG Jincan, LIU Runcong(), WANG Xiaodong()

图11. 锌锅内锌液流速方向与测量装置位置示意图

Fig.11. Flow directions of zinc liquid and the location of the LFV device (αII~αⅤ are the angles between the flow direction of zinc liquid and the measurement direction at II~V)