[an error occurred while processing this directive]
热镀锌工艺中锌液表面流速的在线电磁测量
郑锦灿, 刘润聪(), 王晓东()
Online Electromagnetic Measurement of Molten Zinc Surface Velocity in Hot Galvanized Process
ZHENG Jincan, LIU Runcong(), WANG Xiaodong()
图10. 锌锅内锌液流速现场测试位置和实验结果
Fig.10. Measurement experiment of molten zinc flow (a) industry measurement positions (I~V represent the center positions of LFV device above the zinc bath respectively, while the device is on the position I in this photo, as shown in Fig.3, Δx=30 mm, Δy=200 mm, and h=50 mm)(b) Lorentz force and velocity of molten zinc in the zinc bath due to the electromagn-etic induction