热镀锌工艺中锌液表面流速的在线电磁测量
郑锦灿, 刘润聪(), 王晓东()
Online Electromagnetic Measurement of Molten Zinc Surface Velocity in Hot Galvanized Process
ZHENG Jincan, LIU Runcong(), WANG Xiaodong()

图9. 数值模拟条件下Lorentz力(Fs)与锌板速率(vs)关系数值计算数据及校准曲线

Fig.9. Numerical calculation data and calibration curve of the relationship between Lorentz force (Fs) and vs of zinc plate during numerical calculation