热镀锌工艺中锌液表面流速的在线电磁测量
郑锦灿, 刘润聪(), 王晓东()
Online Electromagnetic Measurement of Molten Zinc Surface Velocity in Hot Galvanized Process
ZHENG Jincan, LIU Runcong(), WANG Xiaodong()

图7. 数值模拟条件下LFV测量装置与固体锌板边缘之间相对位置对测试结果的影响

Fig.7. Effect of relative position between the LFV device and zinc plate on the results during numerical calculation (The horizontal ordinate x=Δy12a, the longitudinal coordinates y=fxfx=6×100%, in which fx is the Lorentz force with different positions at x=Δy12a)