热镀锌工艺中锌液表面流速的在线电磁测量
郑锦灿, 刘润聪(), 王晓东()
Online Electromagnetic Measurement of Molten Zinc Surface Velocity in Hot Galvanized Process
ZHENG Jincan, LIU Runcong(), WANG Xiaodong()

图2. Lorentz力测速仪结构图

Fig.2. Schematic of LFV device (1—support, 2—force sensor, 3—insulation coating, 4—magnet system)