表4 9种对比槽况下两相流场的模拟结果汇总
Table 4 Summary of two-phase flow field simulation results for 9 cases used to compare
CaseLocationCurrent increaseMetal velocity / (m·s-1)Interface deformation / m
%Max.Aver.Min.Max.
11AB: 1~4, 21~24①100.2010.065-0.0450.030
12AB: 1~4, 21~24200.2090.064-0.0530.029
13AB: 5~20②50.1770.067-0.0440.032
14B: 1~4, 21~24③140.1910.067-0.0490.031
15B: 1~4, 21~24280.1960.067-0.0560.030
16B: 1~4, 21~24420.1970.067-0.0610.030
17A: 1~4, 21~24④140.1970.065-0.0440.029
18A: 1~4, 21~24280.2070.063-0.0410.029
19A: 1~4, 21~24420.2150.061-0.0410.030