铝电解槽中局部阴极电流增大对电解质-铝液两相流场的影响
王富强, 刘伟, 王兆文
Effect of Local Cathode Current Increasing on Bath-Metal Two-Phase Flow Field in Aluminum Reduction Cells
WANG Fuqiang, LIU Wei, WANG Zhaowen
表1
物性参数
Table 1
Material properties
Material
Density
kg·m
-3
Viscosity
Pa·s
Conductivity
S·m
-1
Bath
2.13×10
3
2.51×10
-3
0.23×10
3
Metal
2.30×10
3
1.18×10
-3
4.17×10
6