铝电解槽中局部阴极电流增大对电解质-铝液两相流场的影响
王富强1,2, 刘伟2, 王兆文1()
Effect of Local Cathode Current Increasing on Bath-Metal Two-Phase Flow Field in Aluminum Reduction Cells
WANG Fuqiang1,2, LIU Wei2, WANG Zhaowen1()

图10. Case 11、case 12和case 17~case 19的两相流场模拟结果

Fig.10. Simulated two-phase flow fields for case 11 (a1, b1), case 12 (a2, b2), case 17 (a3, b3), case 18 (a4, b4), case 19 (a5, b5) (The current increase locations are shown in square frames) (a1~a5) metal velocity (b1~b5) interface deformation