铝电解槽中局部阴极电流增大对电解质-铝液两相流场的影响
王富强1,2, 刘伟2, 王兆文1()
Effect of Local Cathode Current Increasing on Bath-Metal Two-Phase Flow Field in Aluminum Reduction Cells
WANG Fuqiang1,2, LIU Wei2, WANG Zhaowen1()

图4. 铝液流速测点位置及流速方向

Fig.4. Positions of metal velocity measure points and flow direction