合金化元素对W-Cu体系多类界面特征影响的第一性原理计算
盖逸冰, 唐法威, 侯超, 吕皓, 宋晓艳()
First-Principles Calculation on the Influence of Alloying Elements on Interfacial Features of W-Cu System
GAI Yibing, TANG Fawei, HOU Chao, LU Hao, SONG Xiaoyan()

图7. 图6中Sc和Y偏聚前后各原子间的局域态密度

Fig.7. LDOSs of W1 and W3 before Sc segregation (a), W1 and Sc after Sc segregation (b), W1 and W3 before Y segregation (c), W1 and Y after Y segregation (d) in Fig.6