[an error occurred while processing this directive]
Ti-6Al-4V表面电子束熔覆(Ti, W)C1-x复合涂层的形成及摩擦性能
刘东雷1, 陈情1, 王德2, 张睿2, 王文琴1,4()
Formation and Friction Properties of Electron Beam Cladding (Ti, W)C1-x Composite Coatings on Ti-6Al-4V
LIU Donglei1, CHEN Qing1, WANG De2, ZHANG Rui2, Tomiko Yamaguchi3, WANG Wenqin1,4()

图9. 摩擦实验后基体和涂层表面SEM像及局部放大图

Fig.9. SEM images (a, c, e, g) and local magnifications (b, d, f, h) of substrate and coating surface after friction test
(a, b) substrate (c, d) 12 mA (e, f) 15 mA (g, h) 18 mA