Ti-6Al-4V表面电子束熔覆(Ti, W)C1-x复合涂层的形成及摩擦性能
刘东雷1, 陈情1, 王德2, 张睿2, 王文琴1,4()
Formation and Friction Properties of Electron Beam Cladding (Ti, W)C1-x Composite Coatings on Ti-6Al-4V
LIU Donglei1, CHEN Qing1, WANG De2, ZHANG Rui2, Tomiko Yamaguchi3, WANG Wenqin1,4()

图6. 涂层中各相的形成原理图

Fig.6. Formation schematic diagram of each phase in the coating
(a) schematic illustration of coating cladding(b) partial view of the molten pool(c) reaction diagram of molten pool(d) formation of each phase