Ti-6Al-4V表面电子束熔覆(Ti, W)C1-x复合涂层的形成及摩擦性能
刘东雷1, 陈情1, 王德2, 张睿2, 王文琴1,4()
Formation and Friction Properties of Electron Beam Cladding (Ti, W)C1-x Composite Coatings on Ti-6Al-4V
LIU Donglei1, CHEN Qing1, WANG De2, ZHANG Rui2, Tomiko Yamaguchi3, WANG Wenqin1,4()

图5. 不同复合涂层EPMA点分析位置BSE像

Fig.5. BSE images of EPMA point analysis locations for different composite coatings
(a) 12 mA (b) 15 mA (c) 18 mA