WC-TiC-TaC-Co硬质合金中TaC含量对其显微组织和力学性能的影响
|
|
Effect of TaC Content on Microstructure and Mechanical Properties of WC-TiC-TaC-Co Cemented Carbide
|
|
图4. TaC含量对WC-TiC-TaC-Co硬质合金的密度和硬度的影响 |
Fig.4. Effect of TaC content on the density and hardness of WC-TiC-TaC-Co cemented carbides |
![]() |